Poker burn
Dark coloured marks on the concrete surface. Caused by the insertion vibrating poker brusing the formwork (typically timber) face leaving a scar that is then transferred to the concrete cast surface.

Dark coloured marks on the concrete surface. Caused by the insertion vibrating poker brusing the formwork (typically timber) face leaving a scar that is then transferred to the concrete cast surface.

Lift lines (sometimes referred to as pour lines) appear as colour changes along the boundaries between successive lifts within a pour.

This appears as random dark glossy areas on power trowelled surfaces.

Salt efflorescence appears as a white ‘fluffy’ deposit on the surface of masonry. The deposit can be readily brushed off the surface.

These appear as dark rings around tie-bolt holes. They are caused by localised loss of water at tie-bolt hole in formwork, causing localised changes in the water/cement ratio.

This appears as surface material lost upon striking the formwork.

This appears as a helicopter-blade-like shadow on power-trowelled concrete floor surfaces.

This appears as steps at the surface accompanied by grout loss.

Occasionally, whether precast or in-situ formed concrete, the apparent position of the reinforcement is visible on the formed surface, typically as darker lines. Reinforcement shadow, or perhaps ghosting, is caused by changes in the concrete matrix due to aggregate segregation, localised variation in the water-cement ratio and in the paste/mortar. Any changes in the cement paste affect how it cures and this affects the light and dark tones of the formed surface.

Rain damage on external slabs or those destined to become internal slabs is usually only a surface defect. Although the structural performance of the concrete is unlikely to be affected, clearly, the rain-affected concrete surface may not meet the finish specification and will need to be remedied.