Skip links

Archive

Problems with thin floor coverings (´lino´)

Floor coverings less than 3mm thick are frequently specified to be laid directly onto cement:sand screeds. However, when viewed in cross light, undulations that are unacceptable can often be seen. Special treatment to the surface of the screed may be needed to produce a more acceptable result.

jonnyhough

jonnyhough

Thermal and Shrinkage Cracking in Suspended Slabs

Several papers have been written to deal with individual aspects of shrinkage/thermal movement. However, fully worked examples, especially those which cover each step of the process, are hard to find. The Concrete Society has published a Concrete Advice Sheet describing a conventional floor slab with varying degrees of end restraint and highlights the various correction factors which have been introduced to cover the uncertainties inherent in the method.

jonnyhough

jonnyhough

Crack width and aesthetics

Design codes such as Eurocode 2 (as amended by the UK National Annex), and BS 8110 (withdrawn) limit crack widths to 0.3mm for aesthetic reasons.

jonnyhough

jonnyhough

Autogenous healing

Autogenous healing is the natural process of crack repair that can occur in concrete in the presence of moisture, and the absence of tensile stress. The repair is by a combination of mechanical blocking by particles carried into the crack with the water and the deposition of calcium carbonate from the cementitious material.

jonnyhough

jonnyhough

Damage due to freeze-thaw

Water held in the pores of cement paste will freeze at low temperatures. Ice occupies a bigger volume than water so expansive forces can be generated if the pores are nearly full of water at the time of freezing, i.e. if the concrete is saturated. Damage occurs when the expansive pressure generated by freezing is greater than the local strength of the concrete.

jonnyhough

jonnyhough

Cracks due to alkali-silica reaction

Alkali-silica reaction occurs when the alkaline pour fluid in the cement paste reacts with the minerals in some aggregates. The resulting gel takes up pour solution water and expands, which can disrupt the concrete.

jonnyhough

jonnyhough

Shear cracks

Shear cracks form near the supports of members and are inclined at between about 30o and 45o to the axis of the beam, from the tension face of the member back towards the support. As with flexural cracks, they will be widest at the tension face, reducing in width with distance from the face.

jonnyhough

jonnyhough

Torsion cracks

Pure torsion in a beam is typified by a series of inclined cracks running roughly parallel throughout the length of the member. The cracks basically form a spiral, running up one face of the beam, across the top, down the other side, and back across the bottom to connect with another crack on the first face.

jonnyhough

jonnyhough

Punching shear cracks

Overloading of a slab in punching will lead to cracks forming on the tensile surface of the slab, radiating out from the column. These may be joined to a series of circumferential cracks, located at a distance from the column equal to about three-times the slab thickness. There may be some crushing of the concrete on the underside of the slab at the junction with the column.

jonnyhough