Burnishing of concrete
This appears as random dark glossy areas on power trowelled surfaces.

This appears as random dark glossy areas on power trowelled surfaces.

Lift lines (sometimes referred to as pour lines) appear as colour changes along the boundaries between successive lifts within a pour.

Dark coloured marks on the concrete surface. Caused by the insertion vibrating poker brusing the formwork (typically timber) face leaving a scar that is then transferred to the concrete cast surface.

Delamination is characterised by thin layers of surface mortar becoming detached from the main body of the slab. Concrete Advice Sheet 18 provides an overview of the causes of delamination in concrete floors.

Occasionally, whether precast or in-situ formed concrete, the apparent position of the reinforcement is visible on the formed surface, typically as darker lines. Reinforcement shadow, or perhaps ghosting, is caused by changes in the concrete matrix due to aggregate segregation, localised variation in the water-cement ratio and in the paste/mortar. Any changes in the cement paste affect how it cures and this affects the light and dark tones of the formed surface.

This appears as steps at the surface accompanied by grout loss.

This appears as a helicopter-blade-like shadow on power-trowelled concrete floor surfaces.

This appears as surface material lost upon striking the formwork.

These appear as dark rings around tie-bolt holes. They are caused by localised loss of water at tie-bolt hole in formwork, causing localised changes in the water/cement ratio.

Salt efflorescence appears as a white ‘fluffy’ deposit on the surface of masonry. The deposit can be readily brushed off the surface.