Cover to reinforcement

In nearly all instances, cracks develop at the surface of concrete and are restrained by the tensile reinforcement. If a good bond exists between the concrete and the steel, the width of the crack at the steel will be very small.

jonnyhough

jonnyhough

Cracking in composite concrete/metal decking floor slabs

Composite concrete/profiled steel sheet slabs are a popular form of construction for suspended floor slabs, as they are simple and economical to design and construct. Generally they are found to be satisfactory in service. However, visible cracking is one aspect that occasionally causes problems and complaints from building occupiers. As the majority of composite floors are covered (by finishes, flooring or a raised computer floor) cracking is generally not readily visible. Sometimes the floor use dictates that the surface of the composite slab is left uncovered, e.g. power trowelled floor finishes. It is on exposed floors that cracking can be an issue.

jonnyhough

jonnyhough

Problems with thin floor coverings (´lino´)

Floor coverings less than 3mm thick are frequently specified to be laid directly onto cement:sand screeds. However, when viewed in cross light, undulations that are unacceptable can often be seen. Special treatment to the surface of the screed may be needed to produce a more acceptable result.

jonnyhough

jonnyhough

Bacteria-based self-healing concrete

The concept of bacteria-based self-healing concrete was developed in the Netherlands, has received considerable interest from the press and is the subject of numerous UK research programmes.

jonnyhough

jonnyhough

Mass concrete – a definition

Mass concrete is defined by the American Concrete Institute (ACI 207.1R) as: “any volume of concrete in which a combination of dimensions of the member being cast, the boundary conditions, the characteristics of the concrete mixture, and the ambient conditions can lead to undesirable thermal stresses, cracking, deleterious chemical reactions, or reduction in the long-term strength as a result of elevated concrete temperature due to heat from hydration”.

jonnyhough

jonnyhough

Cold joint in wall between batches

Cold Joints

Cold joints are formed primarily between two batches of concrete where the delivery and placement of the second batch has been delayed and the initial placed and compacted concrete has started to set. The full knitting together of the two batches of concrete under vibration to form a homogeneous mass is therefore not possible, unlike the compaction of two fresh workable batches of concrete. This could be a potential plane of weakness.

jonnyhough

jonnyhough

Large volume concrete pours

In the past large volume concrete pours with low cement content was associated largely with dams to provide weight rather than load-bearing capacity. However, large pours using higher cement contents have become common for general structural applications.

jonnyhough

jonnyhough

Thermal and Shrinkage Cracking in Suspended Slabs

Several papers have been written to deal with individual aspects of shrinkage/thermal movement. However, fully worked examples, especially those which cover each step of the process, are hard to find. The Concrete Society has published a Concrete Advice Sheet describing a conventional floor slab with varying degrees of end restraint and highlights the various correction factors which have been introduced to cover the uncertainties inherent in the method.

jonnyhough

jonnyhough

Crack width and aesthetics

Design codes such as Eurocode 2 (as amended by the UK National Annex), and BS 8110 (withdrawn) limit crack widths to 0.3mm for aesthetic reasons.

jonnyhough

jonnyhough

This website uses cookies to improve your web experience.